January 13, 2018

If you found the model built up or swell, here are some tips for enhancement!

*Especially for the solid / base grid / round-shaped objects 

First, you may wonder why it happens:

-Exposure time too long or,
-Brightness too strong in a short distance(XY50um), resin har...

November 20, 2017

After the print is completed, how should I clean it? Does it require post-cured?

We made a little demo on finishing the print.

1. After taking out the print, please remove the supports in order to clean to back face thoroughly.

2. Bath it in the alcohol for 30sec - 1...

April 9, 2017

With a large resin tank, you will have 14L to fill up the tank. Investing a tank full of resins could be expensive...so we looked for other solution, found these two options and did a long time experiment on both since the day we decided to build a large printer.We wil...